商品の詳細:
|
| 合金: | 7050 | 気性: | T7451 |
|---|---|---|---|
| 直径範囲: | 10mm - 250mm | 長さ: | 1000mm - 5000mm |
| 抗張力: | ≧510MPa | 降伏強さ: | ≧440MPa |
| 伸長: | 9%以上 | 硬度: | ≧145HB |
| 標準: | AMS 4050、ASTM B221、BAC 5431 | 表面: | ミル仕上げ / ポリッシュ |
| 応用: | 航空機の胴体フレーム、翼桁、隔壁構造、着陸装置 | ||
| ハイライト: | 7050-T7451 Stress Resistant,Aircraft Fuselage Grade Bar,High Toughness Zinc Alloy |
||
The 7050-T7451 round aluminum bar is a premium aerospace-grade zinc alloy engineered for superior stress corrosion cracking resistance and high fracture toughness. The T7451 over-aged temper provides an optimal balance of high strength and exceptional durability, making it the preferred choice for critical aircraft structural components where reliability under sustained stress is paramount.
All bars are coated with anti-rust oil and wrapped in waterproof kraft paper, then packed in fumigation-free plywood cases. Standard delivery within 5 working days for stock sizes, 20-30 days for custom production orders.